Hastelloy C276
Physical Properties:
Density: 8.89g/cm3
Melting Point: 1323-1371 0C
Modulus of Elasticity: 205.5kN/mm2
Thermal Conductivity: 11.1 W/m-K
Hardness: HRC90
Electrical Resistivity( 24-1000C) : 11.2 5m/m 0C
Approx Service Temperature: -200 to +4000C
Main Characteristics: Welded structure in atmosphere of strong corrosion, oxidation, reduction or warm sea water situation.
Applications: Applied in aviation, chemical industry and decarbolization in power station.